Abstract
Corrosion is a natural and inevitable problem that is still a challenge in materials design, with regard to achieving greater operational efficiency. In this study, the electrochemical and stress corrosion cracking (SCC) behavior of Cu10Ni alloy in a 3.5% NaCl solution in the presence of different concentrations of sulfide ions were studied. The presence of sulfide ions has been shown to increase the susceptibility of the material to SCC at different strain rates. The addition of glycine (gly) to the test electrolyte increased the time to failure by changing the mode of failure from brittle transgranular cracking to ductile failure. Therefore, gly can be considered as a potential environmentally friendly corrosion inhibitor. The electrochemical measurements showed that gly acts as a mixed corrosion inhibitor. The synergistic effect of potassium iodide (KI) and gly is also investigated. Electrochemical frequency modulation (EFM) and potentiodynamic polarization data are in good agreement with the SCC results.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.