Abstract
As the feature size of integrated circuit (IC) shrinks down to 28nm and below, aluminum (Al) is considered to be one of the suitable gate materials, and cobalt (Co) is considered to be one of the suitable barrier materials. During chemical mechanical polishing (CMP) of the Al-Co gate, galvanic corrosion can occur when two kind of metals with a large open circuit potential (Eoc) difference contact with each other within the device architecture and are exposed to charge conducting CMP slurries. Al is severely corroded as an anode in the presence of Co because the standard electrode potential (E = −1.66 V) is lower than that of Co (E = −0.27 V). In this paper, using the advantages of different materials in adsorption and dissolution of different metal, the effect of glycine and TT-LYK (TT) with different concentrations on galvanic corrosion of Al and Co was studied by potentio dynamic and static polarization measurements with impedance monitoring. The potential different between Al and Co electrodes was significantly reduced for selective adsorption characteristics of the complex formed by glycine with Al and Co significantly reduced the potential difference between Al and Co electrodes. The substances formed by TT with Al and Co can be adsorbed on both surfaces well, and the current difference between Al and Co electrodes can be significantly reduced due to the difference in solubility of the reactants. When glycine and TT were used synergistically, the dynamic corrosion potential (Ecorr) difference between Al and Co electrodes was reduced to 10 mV, and the static Ecorr difference was reduced to 17 mV with glycine concentration of 1000 ppm and TT concentration of 100 ppm. The dynamic corrosion current (Icorr) difference was 0.587μA/cm2, and the static Icorr difference was 2.361μA/cm2.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.