Abstract

Purpose. This study investigated the different effects of quantitative percentages of glass fiber intensity on the transverse strength, maximum deformation, and the modulus of elasticity of acrylic resin. Materials and methods. Fifty-four specimens were formed in a specially designed mold to produce identical specimens in accordance with the manufacturer’s recommendations. Six percentages of glass fiber reinforcement in loose random form were studied. Each glass fiber treatment percentage (0%, 1%, 2%, 5%, 10%, 15%) was related to the total powder/liquid mass. Results. The results indicated that 1% glass fiber treatment enhanced the transverse strength of the tested specimen. Maximum deformation at failure in the tested treatment groups was found to be different. The interaction of glass fiber concentration on fracture strength and deformation was significant ( p < 0.0001). Conclusion. The 1% glass fiber concentration was found to give the best fracture strength and deformation results. Significantly higher glass fiber percentages was found to weaken the resin. (J Prosthet Dent 1998;79:580-4.)

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.