Abstract

ABSTRACTSintering shrinkage of prior cold compacted iron rings with different geometry (height to wall thickness ratio) and green density in the 6.5–7.3 g/cm3 range was investigated. It displays a minimum at an intermediate green density. Axial, tangential and radial shrinkages are different, due to the gradients of green density along the axial and the radial directions. Therefore, the effect of height on shrinkage and its anisotropy is the result of their effect on the stress distribution in the green parts during cold compaction, and the resulting green density and deformation experienced by the powder. Anisotropy decreases on increasing shrinkage.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.