Abstract
Effect of friction pressure on the properties of friction welded hot rolled MA956 iron-based superalloy plate, produced by mechanical alloying, has been investigated. Joining processes were carried out by various friction welding parameters. Tensile strengths and hardness values of the weld interface were determined and the microstructure features of these samples were investigated. Optimum friction pressure for this material was determined.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.