The self-healing capability of cracks plays an important role in improving the durability of concrete. This study investigated the the self-healing capability of mortar with crystalline admixture and fly ash under three conditions. The compressive strength, water absorption, and surface crack pattern were used to evaluate self-healing capability of mortar, and the composition of the healing products was analyzed by x-ray diffraction and scanning electron microscopy. The results indicated that the crystalline admixture could improve the self-healing capability of cementitious materials but caused a negative effect if adding too great an amount of fly ash (≥20%). The specimen that was immersed in water showed favorable self-healing capability of cracks. The healing products in cracks are mainly composed of CaCO3.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.