Floating zone refining of copper under a reduced hydrogen pressure of 0.7 Pa has been carried out. Commercial 99.9999% pure 8-mmdiameter Cu rod was used as a starting material. The purification effect has been examined by the bulk residual resistivity ratio ( RRRB) and glow discharge mass spectrometry (GDMS). The RRRB of the starting material is 3200, and that of refined copper is 22000. Almost all impurities were effectively reduced to near or below their detection limits of GDMS. The removal of S and Se is attributable to the reaction with hydrogen. The marked decrease of Al and Si is ascribed to a convective transportation of alumina and silica inclusions to the surface of the molten zone, and these inclusions are concluded to come from the starting material. This result suggests that trace amounts of Al and Si present as solid solution in starting material can be removed in the same manner by zone melting in a slight oxidizing atmosphere for the first few passes.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.