Abstract

Dissimilar friction stir welding between steels with different carbon contents was carried out by placing the parent materials at two different fixed locations: the advancing side (AS) and the retreating side (RS). The phase transformation and the depth and width of the weld were affected by the fixed location. A smaller weld nugget was formed, and more martensite transformation occurred when the stronger SK5 steel was fixed at AS, compared to that at RS. This variation was attributed to the difference of temperature and materials flow between AS and RS.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.