Abstract

End-linked poly(dimethylsiloxane) (PDMS) networks were prepared in the presence of fumed silica particles with hydroxyl groups at their surfaces. The silica particles were introduced into the polymer solution prior to end-linking. Hydroxyl ended PDMS chains were end-linked via the tetra functional crosslinker, tetraethoxysilane. The filler content varied in the range 0–5wt%. Atomic Force Microscopy was used to image and characterize the silica particles. Swelling, stress–strain and thermoelasticity experiments were performed. The temperature coefficient and the energetic part of the force in uniaxial extension are found to increase with increasing silica amount. This observation is ascribed to effects contributed possibly by the adsorption layer around the silica particles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.