Abstract

Abstract This study describes the effect of FGM coating thickness on apparent fracture toughness (AFT) of a thick-walled cylinder containing two diametrically-opposed edge cracks emanating from the inner surface of the cylinder. The incompatible eigenstrain developed in the cylinder due to nonuniform coefficient of thermal expansion because of cooling from sintering temperature is taken into account. Based on a generalized method of evaluating stress intensity factor (SIF) addressed in a previous study, an approach is developed to calculate AFT. Some numerical results of AFT are presented for a TiC/Al2O3 FGM coating at the inner surface of an Al2O3 thick-walled cylinder.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.