Abstract

Cu-(Fe-Ti)-TiB2 composites were prepared by in situ reaction and vacuum casting with and without ultrasonic vibration. The evolution of the microstructure and mechanical properties of the composite with the variation in Fe element was analyzed. The import of Fe elements could purify the matrix after in situ reaction and the formation of a nanoprecipitated phase, thus improving the strength of Cu-Fe-Ti-TiB2 composites. Meanwhile, compared with the traditional casting process, the Cu-Fe-Ti-TiB2 composites with ultrasonic vibration treatment exhibit uniform TiB2 particle distribution and better properties. The tensile strength and uniform elongation of the composite with a Fe content of 0.7 wt.% reached 511 MPa and 6.02%, increasing by 14.3% and 318% compared to the unalloyed composite, respectively. The tensile strength and uniform elongation of Cu-0.7Fe-Ti-TiB2 composite with ultrasonic vibration treatment increased to 533 MPa and 7.16%, respectively. The TiB2 microscale particles and Fe2Ti nanoscale precipitates with uniform distribution effectively impeded dislocation movement and recrystallization, which improved the tensile strength and stability at elevated temperatures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.