Geopolymers are generally believed to provide good fire resistance due to their ceramic-like properties. Previous experimental studies on geopolymer under elevated temperatures have mainly focused on metakaolin-based geopolymers. This paper presents the results of a study on the effect of elevated temperature on geopolymer paste, mortar and concrete made using fly ash as a precursor. The geopolymer was synthesized with sodium silicate and potassium hydroxide solutions. Various experimental parameters have been examined such as specimen sizing, aggregate sizing, aggregate type and superplasticizer type. The study identifies specimen size and aggregate size as the two main factors that govern geopolymer behavior at elevated temperatures (800 °C). Aggregate sizes larger than 10 mm resulted in good strength performances in both ambient and elevated temperatures. Strength loss in geopolymer concrete at elevated temperatures is attributed to the thermal mismatch between the geopolymer matrix and the aggregates.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.