The impact of electric potential on the dimensional characteristics and membrane surface morphology was investigated in this work. Our study samples comprise hollow fiber (HF) Polysulfone (PS) membrane. Conductive additives have been incorporated within the membrane matrix at the desired predefined concentration. The DC operated electrochemical apparatus consists of graphite anode and stainless steel cathode. The voltage and current density ranges are 2 to 10volts and 0.01 to 1.4mA/mm2 respectively. These investigations have been conducted in alkaline medium at pH=8.5. The results of this work revealed essential changes of hollow fiber (HF) dimensions, including external (DO), internal (DI) and membrane thickness (t). The maximum decrease of DO, DI, and t were 13%, 15%, and 11% respectively at 5volts. EDX analysis showed the maximum sodium ions of about 0.84% on the membrane surface at 2.5volts after 1-hour treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.