Abstract

Polythiophene (PT) was chemically synthesized, undoped using aqueous ammonia and then re-doped using FeCl3 as well as iodine. Doping concentration was changed by changing the duration of doping process. FTIR results indicate the complex formation between PT and each of the dopants. Elemental analysis of FeCl3 doped samples show that as the duration increases concentration of Fe+ ions increases. In case of iodine doped samples atom equivalent of iodine per thiophene unit increases with doping duration. XRD analysis has been used to calculate crystallinity. It is observed that for FeCl3 and iodine (except 120 min) doped samples there is increase in crystallinity due to doping and crystallinity increases with increase in dopant concentration. TGA analysis shows that FeCl3 doped samples are thermally stable compared to iodine doped samples. Results of DTA as well as DSC indicate that Tg values vary with dopant as well as with dopant concentrations. Reduction in Tg values for all FeCl3 doped samples indicate that FeCl3 acts as plasticizer in PT. In iodine doped samples for low values of dopant concentrations Tg increases indicating anti-plasticizer effect whereas for high concentration of iodine, there is decrease in Tg value indicating plasticizer effect of iodine in PT.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.