Abstract

Objective: The aim of this study was to investigate and compare the loading and unloading characteristics of various nickel-titanium (NiTi) and nickel-titanium-copper (NiTiCu) after direct electric resistance heat treatment method (Bender soarer-X equipment). Materials and Methods: Five types of commercial NiTi and NiTiCu orthodontic archwires [NiTi (W&H), NiTi (Ormco), CuNiTi (Ormco), Sentalloy (Tomy) and L&H (Tomy)] underwent heat treatment by the Bender soarer-X equipment and all samples underwent the three point bending tests to analyze their loading and unloading characteristics. Each type of wire was divided into 6 groups with 10 samples per group with one of the groups serving as non-heat treatment control group. The wire composition was analyzed by energy dispersive spectroscopy (EDS) method. Results: The results showed that the loading and unloading characteristics of W&H NiTi and Ormco NiTi after heat treatment were not significantly different from the non-heat treatment groups. But the Tomy Sentalloy, Tomy L&H and Ormco NiTiCu had significantly different results (p<0.05) after heat treatments. The factors which could affect the loading and unloading characteristics were the difference in alloy composition and the condition of heat treatment. Conclusion: Heat treatment increased the loading and unloading force of Tomy L&H and improved the shape forming ability of NiTi wire.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.