Four types of TA2 welded tube-to-tubesheet joints prepared by manual tungsten arc argon-shielded welding technique are studied in this paper. The pull-out tests and low cycle fatigue tests were performed to optimize welded structures of tube and tubesheet. The results show that fractures of welded TA2 tube and tubesheet samples occur at weld zone of TA2 steel tube for the pull-out tests and low cycle fatigue tests. The extension-tubesheet welded joints have the maximum pull-out forces and the best fatigue resistance, and the internal-bore welded joint with 45 deg bevel occupies second place. Fractures are both initiated from weld toe of the outside of tube for the pull-out tests and low cycle fatigue tests. Crack propagates along the direction of 45 deg for the pull-out test. However, crack propagates perpendicularly to the direction of the applied load for low cycle fatigue test, and then fractures immediately parallel to the direction of the applied load. Fatigue striations with a spacing of about 10 μm can be observed on the fatigue crack propagation zone. However, hemispheroidal dimples exist on instant rupture zone.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.