Abstract
Two different origins of natural rubber (NR) from Malaysia; SMR CV60 and Vietnam; SVR 3L filled with 0 and 30phr carbon black (CB) were investigated. Compounds were prepared by a two-roll mill with conventional (CV) and efficient (EV) cure systems. Results obtained show that SVR 3L has higher Mooney viscosity compared to SMR CV60. A different origin of NR has influenced the cure characteristics of rubber compounds. In EV system, SVR 3L compounds showed faster cure rate index (CRI) while in CV system showed contrary results. However, CRI of NR compounds with EV system increased with addition of CB due to high amount of accelerator while CRI in CV system decreased with addition of CB. Torque difference for both NR compounds with each cured system showed similar value. However, mechanical and physical properties were dependent on addition of CB. SVR 3L composites exhibited better tensile strength and recovery from loading force compared to SMR CV60.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.