Abstract In the present study poly(propylene sebacate) (PPSeb) nanocomposites containing 2 wt% of fumed silica nanoparticles (SiO 2 ) or multiwalled carbon nanotubes (MWCNTs), or montmorillonite (MMT) were prepared by in situ polymerization. The thermal degradation of nanocomposites was studied using thermogravimetric analysis (TGA). It was found that the addition of MWCNTs and MMT enhances the thermal stability of the polymer, while SiO 2 nanoparticles do not affect it. From the variation of the activation energy ( E ) with increasing degree of conversion it was found that the decomposition of nanocomposites proceeded with a complex reaction mechanism with the participation of at least two different steps. To evaluate the thermal decomposition mechanisms and mainly the effect of nanoparticles on the thermal decomposition of PPSeb, TGA/FTIR and a combination of TG-gas chromatography–mass spectrometry (TG/GC–MS) were used. From mass ions detection of the formed decomposition compounds it was found that the decomposition of PPSeb and its nanocomposites, takes place mainly through β -hydrogen bond scission and, secondarily, through α -hydrogen bond scission. The main decomposition products were aldehydes, alcohols, allyl, diallyl, and carboxylic acids.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.