Different kinds of hemihydrate calcium sulfate whiskers were fabricated by calcination method under the condition of 115-600 °C. And the density, moisture rate and mechanical properties of composites of gypsum and whisker were studied. The specific strength of composites was investigated. The results show that gypsum boards with whisker calcined at 115 °C and 300 °C have the maximum and minimum densities, which are about 1658 kg/m3 and 1604 kg/m3, respectively. Hydration ability of anhydrous calcium sulfate whisker is the strongest. The values of specific strength of gypsum board reinforced by different types of whiskers suggested that the porosity of the composites changed with the different kinds of whiskers, which agreed well with the moisture rate and mechanical properties.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.