Abstract

Through a series of mechanical properties tests and microstructure observation, the effects of artificial heat treatment (AA), pre-stretching aging (PA) and pre-stretching creep aging (PCA) treatment on the precipitation phase type and mechanical properties of X2A66 aluminum-lithium alloy were studied. The results show that compared with AA, PA treatment promotes the uniform precipitation of high-density T1 phase, so that the yield strength, tensile strength and elongation of the alloy reach 593.4Mpa, 610.8Mpa, 10.7%. Further, the creep aging treatment on the basis of the pre-deformation can further increase the strength (613.6Mpa, 628.9Mpa) of the alloy with a slight decrease in the elongation (10.3%).