AbstractBlending of poly (lactic acid) (PLA)/functionalized gum arabic (FG) in presence of dicumyl peroxide (DCP) presents a simple process to produce film using melt extrusion (recycle time ~ 4 min, screw speed ~60 rpm) at 180°C with tailored characteristics. The FTIR investigation shows that the confirmation of grafting of PLA chains on FG through formation of new C─C linkage. Properties of fabricated films such as morphological, mechanical, UV barrier and contact angle are examined to develop film with improved interfacial interaction, increased toughness, UV–C blocking effect (~95%) and hydrophobicity (~14%). Polarized optical microscopy (POM) studies reveal that PLA/1FG with and without DCP has more crystal density as compared to PLA at 120°C. This melt extrusion permits straightforward, feasible bionanocomposite film and has great potential as a modification with DCP assists to overcome particular drawbacks of FG.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.