Abstract

The research aimed at the composition optimization for diamond-SiC-Si composites. The effect of a porous diamond workpiece was studied on the properties (porosity, density, modulus of elasticity, phase composition) of the product of its siliconization with molten silicon. The lowest porosity and highest modulus of elasticity were observed in the case of using mixed matrices with the maximum size of diamond grains of 250/200 μm for siliconization. The best results in terms of the sound speed (16,600 m/s) and elasticity modulus (860 GPa) were achieved by microwave processing of a composite containing detonation nanodiamonds.