Abstract

The high grade non-oriented electrical steel sheets containing 3.0%Si were manufacturing processed using different cutting techniques, then they were stress relief annealed(SRA), the profiles and textures of the cutting edges were compared before and after annealing, and the magnetic properties of these specimens were tested and compared. The experimental results show that the iron loss of the specimen by water jet cutting is the lowest, but the magnetic induction under the low magnetic field is the highest, the iron loss of the specimen by laser cutting is the highest, but the magnetic induction under the low magnetic field is the lowest. It is necessary to adopt suitable production conditions and minimize the deterioration involved, and the magnetic property can be recovered by SRA effectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.