In the present study, the mechanical properties of geopolymer concrete (GPC) has been investigated. GPC represents a novel technology that is giving significant concern in industrial construction, especially in term of the current emphasis on sustainability. In this study, the NaOH and Na2SiO3 solutions were used as an alkaline solution in all GPC mixes. Na2SiO3 with 10 concentration of molarity, activator-to-FA ratio of 0.4, Na2SiO3/NaOH ratio of 1.75, and two curing regimes viz., ambient curing, and heat curing at 75 °C for 26 h were employed. The experimental results indicated that the geopolymer concrete strengths, modulus of elasticity, and other mechanical properties increased with heat curing as compared to ambient temperature curing. The elastic modulus of GPC was associated with the compressive strengths and similar to those of OPC concrete. Furthermore, the geopolymer concrete mixture requires proper mix proportion and temperature-controlled curing conditions to accomplish good results.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.