The paper describes results of a study of glasses of the type Cux (AsSe1.4 I0.2 )100–x for x =0, l, 5, 10, 15, 20 and 25 at% Cu, by the methods of thermomechanical analysis. Values of the thermal coefficients of linear expansion in solid and visco-plastic phase were determined and the dependence of this parameter on copper concentration was established. The experimental method used enabled the determination of characteristics glass transition temperature and the temperature of the beginning of deformation, and it was found that these parameters increase with increase in the copper content.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.