Abstract
Constant-load indentation creep tests were performed on pure aluminum and aluminum 4 wt% copper at 300 K to assess the influence of indentation depth, copper addition, and heat treatment upon the indentation creep rate. The stress dependence of the average indentation creep rate could be expressed for all the samples tested in terms of a mechanism of obstacle-limited dislocation glide. The calculated activation energy showed the same dependence upon indentation stress for all the conditions investigated. We therefore conclude that the indentation creep rate is limited by dislocation/dislocation interactions regardless of indentation depth, copper addition, or heat treatment. The presence of 4 wt% copper and heat treatment, however changes, the dislocation density, and hence the spacing of the dislocation–dislocation interactions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.