Abstract

In this study, FSSW of DP590 steel was performed using both bare and TiC/TiN coated Si3N4 tool with Ar shielding, and effect of contamination on the microstructure during FSSW was examined. Defect free welds were successfully obtained at all welding conditions. Si, N and O contaminations were clearly found in the weld when bare Si3N4 tool was used without Ar shielding, but the coated tool and Ar shielding could suppress the contaminations. The contaminations caused higher hardness in the vicinity of the pin hole and reduced the weld strength. The present study showed that the prevention of the contaminations could improve the weld strength, especially the cross-tension strength, in FSSW of DP590 steel using Si3N4 tool.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.