Abstract

Polylactide(PLA) films were drawn at various drawing temperature of 65, 90 and 120 °C. The effects of drawing temperature on structural conformation and properties of PLA films were investigated. It was confirmed that the PLA films at drawing temperature of 65 and 90 °C were composed of α′ phase crystal form. The strain-induced crystallization and molecular orientation increased with increasing the draw ratio, which result in improving the mechanical and thermal properties of α′ phase PLA films. However, at drawing temperature of 120 °C, the strain-induced crystallization and molecular orientation of PLA films were not distinctly detected. It was supposed that the rate of the chain relaxation was faster than chain orientation and strain-induced crystallization during uniaxial drawing process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.