Abstract
The effect the conditions of preparing thermoelectric solid solutions of Bi0.5Sb1.5Te3 + 0.06 wt % Pb by hardening from the liquid state with subsequent hot pressing have on their thermoelectric properties is studied. It is found that the optimum thermoelectric quality factors are achieved at a 2200–2800 rpm rate of copper disc rotation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Bulletin of the Russian Academy of Sciences: Physics
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.