Abstract
Purpose: The study was to determine the mechanical properties of hypo-eutectic silumin AlSi12 modified with Sr or Al-Sr alloy slow or fast cooled and in the form of a strip or powder. Design/methodology/approach: The experiment performed on EN AB-AlSi12 hypoeutectic alloy. Aluminium and strontium was melted and next fast cooled to room temperature or cooled on a metal plate at rates about 200°C/s. This enabled to produce a different components, which were powdered immediately before adding to the alloy or used as a strip. The scope of this paper was to verify the cooling effect of Sr-Al modifiers and its form (powder or strip) on the microstructure and mechanical properties the AlSi12 alloy. Findings: The use of fast cooled Al-Sr alloy in the modification process and/or powdered alloy contributed to a further increase mechanical properties AlSi12 alloy. Research limitations/implications: The modification alloys with fast cooled powdered modifier are attractive for future research. Practical implications: Widely presented books and research papers on the silumin treatment give not a lot of contents on the effect treatment fast cooled alloy in the form of a strip or powder. Originality/value: The original value of the paper is comparison Sr and Al-Sr alloy modifiers slow and fast cooled and used as a powder or strip.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Achievements in Materials and Manufacturing Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.