Abstract

In this study, low cycle fatigue behavior of Zircaloy-4 alloy cladding tube manufactured by cold Pilger rolling and annealing was investigated at room temperature. Results revealed that fatigue cracks initiated toward the marked side on clamped position i.e. on outer wall of the tube. Besides, substantial microstrain and dislocation developed on the out wall surface of the tube during manufacturing stage, which playing a key role in the fatigue crack initiation of the specimens. Meanwhile, effects of grain size and texture of the out wall surface, inner wall surface and cross section remained almost indifferent in this regard.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.