Abstract
Activated carbon honeycombs (ACHs) were prepared by extrusion of honeycombs from a mixture of coal, coal tar, bean oil, methylcellulose and water, followed by carbonization and steam activation. Three Chinese coals, Qujing, Shenfu and Datong, were used as carbon precursors. The ACH monoliths obtained were characterized by N2 adsorption,thermo-gravimetry and compression tests. Results show that both coal rank and activation time have great a impact on the pore size distribution and mechanical strength. The ACHs from Datong obtained under optimum conditions have the highest BET surface area(884m2/g), the highest ignition temperature (535℃) and the highest mechanical strength(13MPa) among the three coals. The mechanical strength of the ACH monoliths decreases with increasing macro-pore volume. The ignition temperature is hardly affected by ash content but decreases with increasing volatile content.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.