Abstract

Commercial α-Al2O3 and Y2O3 powders with 0.5 wt% TEOS were used to fabricate transparent polycrystalline YAG ceramics by reactive spark plasma sintering. The powder mixtures were dispersed with dispersants of PAA and citric acid in aqueous slurry. YAG specimens sintered at 1400 °C for 3 min were used to investigate the effect of processing parameters on the microstructure and the optical properties. It is found that a pretreatment of the powders mixture with 0.6 wt% citric acid can significantly improve the microstructure homogeneity of the as-sintered YAG ceramics. After post-annealing in wet air, the specimen sintered from the treated powders mixture was transparent, while the specimen from the untreated powders mixture was hazy. The effects of citric acid for this were investigated in this paper.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.