In this paper, terephthalaldehyde (TPA) is proposed as non-toxic and non-volatile gelatin cross-linker. Optimal cross-linking parameters (TPA/gelatin ratio, temperature) were first determined from in situ rheological measurements on gelatin solutions and from chemical tests with 2,4,6-trinitrobenzenesulfonic acid (TNBS assays) on gelatin gel. The highest cross-linking ratio was achieved for a concentration of 0.005g TPA/g gelatin at 60°C. The impact of TPA cross-linking on gelatin membrane functional properties (water swelling ratio, water vapor sorption and mechanical properties) was measured. TPA cross-linking increased 17 times the liquid water resistance duration of gelatin films, and delayed the entry of vapor water in the polymer matrix for 7 days, indicating that TPA increased the hydrophobic character of the gelatin matrix.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Biological Macromolecules
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.