Abstract

Er:NaY(WO4)2 and Er:Yb:Ce:NaY(WO4)2 crystals were grown by the Czochralski method. Er:Yb:NaY(WO4)2, Er:Ce:NaY(WO4)2, and Yb:NaY(WO4)2 crystal powders were synthesized by means of the solid-state reaction. The spectroscopic properties of the crystals were investigated, including the absorption and fluorescence spectra and fluorescence decay. The energy transfer efficiency from Yb3+ to Er3+ in Er:Yb:NaY(WO4)2 and Er:Yb:Ce:NaY(WO4)2 was calculated and analyzed. End-pumped by a diode laser at 970 nm in a hemispherical cavity, a 1.84 W quasi-continuous-wave laser around 1.55 μm with a slope efficiency of 17% and an absorbed pump threshold of 1.60 W was achieved in a 1.04 mm thick c-cut Er:Yb:Ce:NaY(WO4)2 crystal. The results show that the Er:Yb:Ce:NaY(WO4)2 crystal with high Ce3+ doping is a candidate for gain medium of low threshold 1.55 μm laser.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.