Abstract

The billets of AlMg0.9Si0.7 alloy, which were cast through the direct chill (DC) casting process of low superheat, were analyzed to study the effect of casting velocity on the surface quality and the morphology of primary α grains. The results show that the nucleating quantity of primary α grains in the melt is increased obviously due to the low pouring temperature during DC casting of low superheat. The suitable temperature gradient in front of the solid-liquid interface is obtained by changing the casting velocity, and the dendritic growth of the primary α grains is inhibited effectively. The billet of AlMg0.9Si0.7 alloy with smooth surface and homogeneous, fine rosette-shaped grains is obtained at the velocity of 130mm/min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.