Abstract

In this paper, the as-cast microstructure, microsegregation, and mechanical properties of GH4151 superalloys with a carbon addition were studied by scanner electron microscopy (SEM), transmission electron microscope (TEM), electron probe microanalysis (EPMA), differential thermal analyzer (DSC), and electron backscattered diffraction (EBSD). The results show that the solid solution effect of carbon in alloys is limited, the addition of C from 0.01 to 0.08 ​wt% significantly refines the secondary dendrite spacing(SDAS) from 61.7 to 57.4 and 51.8 ​μm. Due to the influence of thermal solutal convection, the most severe segregation is found in the C-0.04 alloy, and the solidification ranges of C-0.01, C-0.04, and C-0.08 alloys are 87 ​°C, 96 ​°C, and 83 ​°C, respectively. Owing to the reduced solidification pores and formed finely dispersed carbides, C-0.04 shows excellent ultimate tensile strength (442 ​MPa) and superior total elongation (1.368%) at 1100 ​°C much better than that of C-0.01(130.7 ​MPa, 0.085%) and C-0.08(248 ​MPa, 1.026%).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call