The effect of TaC, VC, Cr3C2, NbC, and TiN additives on the strength and hardness of sintered TiC-Mo2C-Ni hard metals was studied. The additive powder was mixed separately with the TiC-Mo2C-Ni base powder. The powder mixtures were then compacted and sintered in a vacuum. Experimental results showed that the transverse rupture strength of sintered hard metals was effectively promoted by adding the VC and TiN powders, respectively. However, no additives increased the hardness value of the base materials.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.