Abstract

Thermal treatment technology considerably affects the harmlessness of fly ash (FA), but highly toxic heavy metals, such as Cr, attract considerable attention. In this study, we investigated the influence of CaO dosage at 600°C-1200°C on the curing effect of Cr during FA thermal treatment based on the combination effect of CaO. Static, dynamic, and continuous sequential leachings were performed for the sintered products. Results showed that the leaching concentration of Cr decreased by approximately 91% when CaO dosage was 8.57%, and the difference in the residual state was the main reason for the difference in the leaching behavior of Cr. The proportion of the residual state in the sintered products increased from 35.16% to 64.01%. The transition between Cr2O3, Cr5O12, and CaCr2O4 is the fundamental reason for the leaching behavior of Cr and the change in the residual state. This study provides a scientific basis for preventing and controlling heavy metal pollution and optimizing environmental supervision in the FA thermal treatment process.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call