Abstract

The effect of Ca addition on the as-cast microstructure and creep properties of Mg-5Zn-5Sn magnesium alloy was investigated. The results indicate that adding 1.0 wt.% Ca to Mg-5Zn-5Sn alloy can effectively refine the as-cast microstructure of the alloy, and the CaMgSn phase with high thermal stability is formed in the alloy. In addition, adding 1.0 wt.% Ca to Mg-5Zn-5Sn alloy can also improve the creep properties of the alloy. After adding 1.0 wt.% Ca to Mg-5Zn-5Sn alloy, the second creep rate of the alloy at 150°C and 50 MPa for 100 h decreases from 4.67 × 10−8 to 1.43 × 10−8 s−1. The strengthening mechanism is mainly attributed to the microstructural refinement and the formation of CaMgSn phase.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.