Abstract
Coal minerals and tetraethoxysilane were used to prepare SiC by microwave heating. Different C:SiO2 ratios of raw mixed powders were selected to investigate changes in the heating behavior and photoluminescence property. The prepared samples were characterized by X-ray diffraction (XRD) Raman Field-emission scanning electron microscopy (SEM) and X-ray fluorescence spectrophotometer. It was found that distinct heating behavior appeared for different C:SiO2 ratios, including the time taken to reach ~600 °C, performance of the thermal runaway, and heating rate. The changes in the complicated heating behaviors are determined by different microwave coupling, microwave plasma, and E-field intensification effects within samples with different C:SiO2 ratios. When the molar ration of carbon and silicon is 5:1, the intensity of light emission reaches maximum.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.