Abstract

This study aims to systematically investigate the influence of boron (0–3.0 wt % B) on microstructure and abrasive wear characteristics of high chromium based multi-component white cast iron (Hi-Cr MWCI).As result, the microstructure is mainly composed of martensite matrix and carborides such as M7(C, B)3, M2(C, B), M23(C, B)6. At low load, B can increase the wear resistance of Hi-Cr MWCI owing to the higher volume fraction of M2(C, B). However, it reduces the wear resistance of material due to low the fracture toughness of primary M7C3 or M7(C, B)3 at high load. Therefore it can be concluded that B addition can improve the abrasive wear resistance of Hi-Cr MWCI at low load, but, the opposite tendency will occur at high load.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.