In this study, the physical and mechanical behaviors of geopolymers prepared by using different amounts of silica fume and calcium hydroxide as binding materials, acidic pumice as fine aggregate and waste aluminium particles as air-entraining agent were investigated. Test results showed that binder types, amount of binders and alkali activator (sodium hydroxide) significantly affected the physical and mechanical behavior of geopolymer specimens. Bulk density, compressive and flexural strength decreased with the higher alkali activator content. Addition of waste aluminium particles led to decrease in bulk density and strength due to the some extent of entrained air. In the case of same alkali activator content, compressive and flexural strength increased with increase in silica fume and calcium hydroxide up to a certain level.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.