Abstract

The effect of various benzoic acids on the precipitation of barite (BaSO4) and calcite (CaCO3) was investigated. The acids varied in the number of carboxylate groups, from dibenzoic acids (phthalic, isophthalic, and terephthalic) through to the hexabenzoic acid (mellitic acid). It was found that the stereochemistry of the dibenzoic acids was important, as was the pH of the solution (trimesic acid was used as a test case and showed that greatest inhibition was achieved with all carboxylate groups deprotonated). Interestingly, for both the calcite and barite systems, mellitic acid was found to be both a potent inhibitor and a significant crystal growth modifier. In the case of barite, the presence of mellitic acid produced nanoparticles that agglomerated. The nanoparticles were found to be ∼20 nm in size from X-ray diffraction (XRD) line width analysis and 20−50 nm from transmission electron microscopy (TEM). Humic acid was also tested and found to form bundled fibers of barium sulfate.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.