Abstract

To avoid slag sticking onto the snorkel during CAS-OB ladle refining process, B2O3-CaO(mass ratio equals 1:1) and CaF2-CaO(mass ratio equals 1:1) were respectively employed as modifiers added to decrease the viscosity of ladle slag. The rotary cylinder method was adopted in the viscosity measurements. The results showed that the modifiers could decrease the viscosity of ladle refining slag remarkably. At 1500°C, the viscosity of ladle slag without any modifiers is about 6.0 Pa·s. But by adding more than 10mass% CaO-B2O3 or CaO-CaF2, the slag viscosity at 1500°C could be decreased lower than 1.0 Pa·s. The mechanism of modifiers decreasing the slag viscosity was analyzed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.