Abstract
Ti-2Mn-2Sn-xB (x = 0, 0.3, 0.5, 1, and 2 wt%) was produced in this research employing conventional powder metallurgy methods (cold pressing and sintering). The densification behavior, microstructure, and mechanical properties of Ti-2Mn-2Sn alloy caused by the addition of B were systematically studied. The outcomes indicated that the inclusion of B element can inhibit the densification behavior of Ti-2Mn-2Sn alloy. The morphology of microstructure eventually shifts from plate to equiaxial with the inclusion of B element. When the B element is less than 2 wt%, the strength of the sample exhibits an upward trend, which is mainly attributable to the combined effect of grain refinement and the presence of small amounts of TiB.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.