Abstract
Using anti-COVID-19 mouthwashes has become necessary to reduce acute respiratory syndrome coronavirus 2 (SARS-CoV-2) transmissions. Resin-matrix ceramic (RMCs) materials that are exposed to mouthwashes may affect the bonding of repaired materials. This research was performed to assess the effects of anti-COVID-19 mouthwashes on the shear bond strengths (SBS) of RMCs repaired with resin composites. A total of 189 rectangular specimens of two different RMCs (Vita Enamic (VE) and Shofu Block HC (ShB)) were thermocycled and randomly divided into nine subgroups according to different mouthwashes (distilled water (DW), 0.2% povidone-iodine (PVP-I), and 1.5% hydrogen peroxide (HP)) and surface treatment protocols (no surface treatment, hydrofluoric acid etching (HF), and sandblasting (SB)). A repair protocol for RMCs was performed (using universal adhesives and resin composites), and the specimens were assessed using an SBS test. The failure mode was examined using a stereomicroscope. The SBS data were evaluated using a three-way ANOVA and a Tukey post hoc test. The SBS were significantly affected by the RMCs, mouthwashes, and surface treatment protocols. Both surface treatment protocols (HF and SB) for both RMCs, whether immersed in anti-COVID-19 mouthwash or not, improved the SBS. For the VE immersed in HP and PVP-I, the HF surface treatment had the highest SBS. For the ShB immersed in HP and PVP-I, the SB surface treatment had the highest SBS.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.