Abstract

The effect of annealing treatment on the structure and electrochemical properties of LaNi4.5Co0.25Al0.25 alloy was studied by X-ray diffraction (XRD), scanning electron microscopy (SEM) and electrochemical measurement. XRD results show that the matrix phases are still LaNi5 (hexagonal CaCu5 type structure) but the intensity peaks become sharper after heat treatment. Electrochemical experiments at 301 K indicate that annealing treatment can significantly improve the discharge capacity and cyclic stability of LaNi4.5Co0.25Al0.25 alloy at suitable treatment condition. The alloy has the best discharge capacity (324.4 mAg-1) due to its composition homogenization after heat treatment at 1373 K/8 h, while the best capacity retention is about 80.12 % because of lower expansion rate and better anti-pulverization ability after heat treatment at 1273 K/8 h.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.