Nanostructured WO3 films are prepared on p-Si substrate by facing target sputtering (FTS) method with sputtering pressure, 0.1Pa and 200W. The sample is annealed at 850C in air with 5C/min. The as-deposited and annealed WO3 films have been characterized by the Grazing incidence X-ray diffractometer, Field emission electron microscopy, and Ultraviolet-visible spectrophotometer. The surface morphology of the WO3 films strongly depends on the annealing temperature. An average diameter of the WO3 nanorod is 5-6μm long and 800nm diameter. It is revealed from optical study that the band-gap energy of WO3 films is around 2.85eV. The surface morphology of nanostructured WO3 films has been discussed with the increase of annealing temperature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.