Abstract

N-type thermoelectric bismuth telluride (Bi2Te3) was deposited on virgin carbon fibre (VCF) and recycled carbon fibre (RCF) substrates by electro-deposition. The effects of annealing on the surface morphology and the Seebeck coefficient of the Bi2Te3 films were investigated. A nearly stoichiometric N-type Bi2Te3 was obtained from an electrolyte of 8 mM of Bi(NO3)3.5H2O and 10mM of TeO2, which exhibited the highest Seebeck coefficient of -20.1 µV/K and -13.0 µV/K for VCF and RCF individually. The effect of varying annealing temperature (548.15 K and 623.15 K) and annealing time (2 and 3 h) was carried out only on nearly stoichiometric N-type Bi2Te3 that revealed improvement in Seebeck coefficient up to 1.51 times and 1.24 times for VCF and RCF at 623.15 K for 2 h.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.